The service was prompt but i found difficulty in the fibreglass drying. I still have some damp. I put plenty of hardner, running out I used so much. It should have gone off in half hour. The general purpose resin I do not think it is right for the boat and the fibre glass matting was not very well knitted together, a bit thin in places and it when cutting it just shredded in parts. But I managed by doubling up in parts where thin. Otherwise I am very pleased with your service. The resin etc is bot boat repair and molding parts for my little boat. I have a 20ft boat to fibreglass up and will need at least 10kg of resin and suitable catalist for it to set hard. I always give myself a half hour going off time and should be a couple of hours setting hard. A full day totla setting after that. Thank you.